Fire Retardancy of Fire-retardant-impregnated Wood after Natural Weathering II.(dagger) Degradation behavior of fire-retardant-impregnated wood used with water-soluble fire retardant

Kawarasaki, M; Hiradate, R; Hirabayashi, Y; Kikuchi, S; Ohmiya, Y; Lee, J; Noaki, M; Nakamura, N

Kawarasaki, M (corresponding author), Hokkaido Res Org, Forest Prod Res Inst, Asahikawa, Hokkaido 0710198, Japan.

MOKUZAI GAKKAISHI, 2020; 66 (1): 31

Abstract

Wood samples treated with water-soluble fire retardants were exposed to natural weathering for up to 36 months at three locations in Japan. Three leve......